Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 17.92 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 17.92 GPa
2599 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66
LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b..
Flexural Modulus 17.92 GPa
2599 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp DCL36 PC
LNP LUBRICOMP* DCL36 is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP fo..
Copyright © lookpolymers.com All Rights Reserved