Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 170.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.172 GPa
170.0 ksi
ISO METHOD 178
NYCOA 2012 Copolymer Nylon
easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc.
Flexural Modulus 1.172 GPa
170.0 ksi
ASTM D790
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer  (discontinued **)
Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesCharacteristics:..
Flexural Modulus 1.172 GPa
170.0 ksi
ASTM D790
Eastman Tenite 307A4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Modulus 1.172 GPa
170.0 ksi
ASTM D790
Eastman Tenite 307E4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Flexural Modulus 1.172 GPa
170.0 ksi
ASTM D790
Eastman Tenite 380A3V32818 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Flexural Modulus 1.172 GPa
170.0 ksi
ASTM D790
Eastman Tenite Propionate 307A2R30018 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
Flexural Modulus 1.172 GPa
170.0 ksi
ASTM D790
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
Flexural Modulus 1.172 GPa
170.0 ksi
ASTM D790
Eastman Tenite Propionate 380A2R30018 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
Flexural Modulus 1.172 GPa
170.0 ksi
ASTM D790
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer
Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55..
Flexural Modulus 1.172 - 1.724 GPa
170.0 - 250.0 ksi
Polypropylene; ASTM D790M
DSM Somos® 9120
The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp..
Copyright © lookpolymers.com All Rights Reserved