Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.724 GPa | 1700.4 ksi | ASTM D-790 |
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by .. |