Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.91 GPa | 1727 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RX00327 PA 66 LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural. |