Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 18.02 GPa | 2614 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific) LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 18.02 GPa | 2614 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Flexural Modulus | 18.02 GPa | 2614 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Flexural Modulus | 18.02 GPa | 2614 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 18.02 GPa | 2614 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |