Mechanical Properties Metric English Comments
Flexural Modulus 12.57 GPa
1823 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66
LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead.
Flexural Modulus 12.57 GPa
1823 ksi
ASTM D790
Covestro Baydur® STR/C-410 IMR Polyurethane Composite SRIM Foam, 60% Glass Filled, MDI-based 2-Component Liquid System
Contains continuous strand fiberglass mat.0.126 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer ..