Flexural Modulus 0.137 GPa
19.9 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 8620 BLK
Formulated TPE compound is based on Shell's Kraton G resin and is widely used in automotive applications exhibiting a wide temperature range, replacing in many applications conventional thermoset ru..