Flexural Modulus 19.92 GPa
2889 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS (Asia Pacific)
LNP* Lubricomp* OCP36 is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, Lubricants, Bearing Grade. Added features of this material include: Internally Lubricated, Electric..
Flexural Modulus 19.92 GPa
2889 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear
LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Bearing Grade, Electrically Conductive, Wear R..
Flexural Modulus 19.92 GPa
2889 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing Bearing Grade, Carbon Fiber, Lubricants. Added features of this material include: Electrically Conductive.