Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR43 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
PolyOne Edgetek® LC-30GF/000 LCP (Liquid Crystal Polymer), 30% Glass Reinforced, Hi-Temp
(discontinued **)< Information provided by PolyOne™ Corporation |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp RFN18SXZ PA 66 LNP LUBRICOMP* RFN18SXZ is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Ameri.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Techmer ES HiFill® PPA GF45 HS L X 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat Stabilizer, Mold Release and LubricantFeatures: Heat Stabilized, Gold Mol.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Techmer ES Statiblend® PPS GF35 SS7 BK 35/7% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel Fiber, 35/7% Filler by WeightUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Ashley Polymers Ashlene® PE128 PET Polyester, 45% Glass Reinforced PET Polyester, with 45% glass reinforcement.Data provided by the manufacturer |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |