Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.32 GPa | 191 ksi | ASTM D790 |
Iran Petrochemical (PCC) 52511 High Density Polyethylene 52511 is a HDPE copolymer injection molding grade for applications requiring a good balance between physical properties and flowability, like housewares and toys.Application: houseware, injection m.. |
|||
Flexural Modulus | 1.32 GPa | 191 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PD701 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.32 GPa | 191 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® SM840 Polypropylene impact copolymer Titanpro® SM840 is an extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvant.. |
|||
Flexural Modulus | 1.32 GPa | 191 ksi | Tangent Method 1; ASTM D-790 |
Bapolene® 3262 Polyethylene, Injection Grade Narrow molecular weight distribution injection molding resin. This resin offers intermediate flow, excellent ESCR, excellent impact and good warp resistance. This product meets FDA standards for f.. |
|||
Flexural Modulus | 1.32 GPa | 191 ksi | Secant @ 1% strain; ASTM D-790 |
Bapolene® PP5026 Polypropylene, Extrusion/Injection Grade Polypropylene extrusion impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA regulation 21 CFR .. |
|||
Flexural Modulus | 1.32 GPa | 191 ksi | ASTM Test |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |