Flexural Modulus 1.336 GPa
193.7 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CH042V Polypropylene, Homopolymer, Extrusion, Sheet
COPYLENE™ CH042V is a polypropylene homopolymer resin often used in extrusion applications. Replacement alternative to Pro-fax® HL561KInformation provided by Phillips 66.