Mechanical Properties Metric English Comments
Flexural Modulus 13.33 GPa
1933 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI
LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this material include: Electrically Conductive.