Mechanical Properties Metric English Comments
Flexural Modulus 1.339 GPa
194.2 ksi
1% Secant; ASTM D790
Flint Hills P4C5Z-027 Homopolymer Polypropylene
Homopolymer, UL certified, USP Class VI certified, and FDA compliant.Features: controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now pro..