Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.093 GPa | 303.6 ksi | ASTM D790 |
E-Polymers TEKANATE® G7013 General Purpose Easy Molding Polycarbonate Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows .. |
|||
Flexural Modulus | 2.093 GPa | 303.6 ksi | ASTM D790 |
E-Polymers TEKANATE® G7013FR General Purpose Easy Molding Flame Retardant Polycarbonate Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows .. |