Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Asia Pacific) Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Asia Pacific) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 13 mm/min; ASTM D790 |
PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Asia Pacific) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® X0700 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | ASTM D790 |
Aaron Industries AAROLENE® ARPS GP 100-1 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Flexural Modulus | 2.12 GPa | 308 ksi | ASTM D790 |
Aaron Industries AAROLENE® ARPS MI 100-2 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX2071T PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |