Polymer Property : Flexural Modulus = 2.203 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.203 GPa
319.5 ksi
ASTM D790
NYCOA 1417 HS Heat Stabilized, Impact Modified Nylon 6 Resin
NYCOA 1417 HS is a heat stabilized and impact modified Nylon 6. This medium viscosity resin was developed for injection molding and extrusion processes for applications requiring improved toughness,..