Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS Automotive applications: High impact and ductility to -22F for interior trim and instrument panel applications. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | ISO 178 |
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7691 PC UV stabilized clear polycarbonate formula for internal uses only. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Asia Pacific) Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Flexural Modulus | 2.23 - 3.31 GPa | 323 - 480 ksi | Average value: 2.68 GPa Grade Count:11 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON FX98501 PE LNP* STAT-KON* FX98501 is a compound based on Polyethylene resin containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | ASTM Test |
Styrolution Luran® S 757 G ASA Luran S 757 G is an easy flowing injection molding ASA grade with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon DS0029 PC LNP STAT-KON* DS0029 is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NX11302 PC+ABS (Asia Pacific) This is a PC/ABS compound with colorable, good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2637 PPE+HIPS (Asia Pacific) |
|||
Flexural Modulus | 2.23 GPa | 324 ksi | ASTM D790 |
Engineered Polymer Solutions PPE/PA 9100 PPE/Nylon Alloy. Natural and colors available. Injection molding grade. Uses: General Purpose, paintable, plate-ableInformation provided by Engineered Polymer Solutions. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | ISO Data |
BASF Ultramid® B29 HM 01 PA6 (Dry) Ultramid B29 HM 01 is a medium viscosity , heat stabilized, PA6 universal wire jacketing resin offering excellent performance through the range of THHN, THWN, and TFFN constructions. It possesses a.. |
|||
Flexural Modulus | 2.23 GPa | 323 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® A0501 PPE/PA AutomotiveInformation provided by Asahi Kasei |