Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.252 GPa | 326.6 ksi | ASTM D790 |
KKPC Kuhmo HI 450S High Gloss HIPS Key features: High-gloss Common Uses: Portable CD-case, air conditioner cases.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impac.. |
|||
Flexural Modulus | 2.252 GPa | 326.6 ksi | ASTM D790 |
KKPC Kuhmo HI 450PG High Gloss HIPS Common Uses: Monitor swivels, washers.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resistance and heat-resistance.Data pr.. |