Mechanical Properties Metric English Comments
Flexural Modulus 2.374 GPa
344.3 ksi
ASTM D790
E-Polymers TEKAMID® JN2 PPE+PA66 Un-reinforced Chemical resistance PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..