Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2.40 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0165 GPa
2.40 ksi
2% Secant, in accordance with ASTM D638; ASTM D790
M. Holland Company MAGMA® Magmalene Polyalphaolefin  (discontinued **)
High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessUses: BlendingProcessing Method: Injection MoldingInformation provided by M. Holland.
Flexural Modulus 0.0165 - 0.758 GPa
2.40 - 110 ksi
Average value: 0.383 GPa Grade Count:55
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Flexural Modulus 0.0165 GPa
2.40 ksi
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System
Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru..
Flexural Modulus 0.0165 - 1.93 GPa
2.40 - 280 ksi
Average value: 0.857 GPa Grade Count:16
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..
Copyright © lookpolymers.com All Rights Reserved