Polymer Property : Flexural Modulus = 2.482 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.482 GPa
360.0 ksi
ASTM D790
KYDEX® 311 Co-Extruded High Impact Fire-Rated Thermoplastic Sheet
Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent..
Flexural Modulus 2.482 GPa
360.0 ksi
ASTM D790
KYDEX® 311 MB Co-Extruded High Impact Fire-Rated Thermoplastic Sheet with Microban® Antimicrobial
Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent..
Flexural Modulus 2.482 GPa
360.0 ksi
ASTM D790
KYDEX® 321 Co-Extruded High Impact Fire Rated Sheet
Features:Metallic cap, black, gray or off-white substrateThickness ranging from 3.18 mm to 8.9 mmTextures: P-3 Velour Matte and P-C Level HaircellImpact resistantEasy to form with good part definiti..
Flexural Modulus 2.482 GPa
360.0 ksi
ASTM D790
KYDEX® 331/331d Co-Extruded High Impact Fire Rated Thermoplastic Sheet with Weatherable Acrylic Film Cap
KYDEX® 331 is a co-extruded high impact fire rated thermoplastic sheet with a weatherable cap that offers superior performance for thermoforming. It can also be used as an impact resistant surfa..