Flexural Modulus 2.485 GPa
360.4 ksi
ISO 178
Brueggemann Chemical Nyrim® 1000 (Dry)
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec..