Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2.51 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.51 GPa
364 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics GELOY HRA222 ASA
GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. Use for exterior/interior electrical applications requiring UV resistance.
Flexural Modulus 2.51 GPa
364 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics GELOY HRA222 ASA (Asia Pacific)
GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. Use for exterior/interior electrical applications requiring UV resistance.
Flexural Modulus 2.51 GPa
364 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East)
GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by..
Flexural Modulus 2.51 GPa
364 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics GELOY HRA222 ASA+PC (Europe-Africa-Middle East)
GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.
Flexural Modulus 2.51 GPa
364 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics GELOY HRA222F ASA+PC
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application..
Flexural Modulus 2.51 GPa
364 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific)
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application..
Flexural Modulus 2.51 GPa
364 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East)
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured..
Flexural Modulus 2.51 GPa
364 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics GELOY XP4034 ASA+PC
Available in a wide range of colors. Recommended for unpainted exterior/high heat/high impact applications.
Flexural Modulus 2.51 GPa
364 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics GELOY XP4034 ASA+PC (Asia Pacific)
Weatherable, injection moldable ASA+PC blend. In a wide range of colors. Recommended for unpainted exterior/high heat applications.
Flexural Modulus 2.51 GPa
364 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.
Flexural Modulus 2.51 GPa
364 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® OQ1060 PC Copolymer
Optical quality, high flow, high purity Polycarbonate copolymer resin with reduced oxygen transmission for advanced DVD applications such as Limited Play DVD.This data was supplied by SABIC-IP for t..
Flexural Modulus 2.51 GPa
364 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific)
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.
Flexural Modulus 2.51 GPa
364 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg..
Flexural Modulus 2.51 GPa
364 ksi
clear casting
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin
TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA..
Flexural Modulus 2.51 GPa
364 ksi
ISO 178
FKuR Kunststoff Bio-Flex® F 6611 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Flexural Modulus 2.51 GPa
364 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East)
Flexural Modulus 2.51 GPa
364 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM DU242 PEI
Enhanced low temperature impact, high flow Polyetherimide blend. ECO Conforming.
Flexural Modulus 2.51 GPa
364 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DX04490 PC
LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Flexural Modulus 2.51 GPa
364 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON AD000 ABS
LNP* STAT-KON* AD000 is a compound based on ABS containing Carbon. Added feature of this grade is: Electrically Conductive.
Flexural Modulus 2.51 GPa
364 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Flexural Modulus 2.51 GPa
364 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Flexural Modulus 2.51 GPa
364 ksi
clear casting
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin
TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA..
Flexural Modulus 2.51 GPa
364 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA TW-18B1
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.51 - 2.59 GPa
364 - 376 ksi
ASTM D790
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon
Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast..
Flexural Modulus 2.51 GPa
364 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Flexural Modulus 2.51 GPa
364 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific)
LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Flexural Modulus 2.51 GPa
364 ksi
2.6 mm/min, 100 mm span; ASTM D 790
SABIC Innovative Plastics Noryl EN212 PPE+PS
Extrusion grade. 212F (100C) DTUL. UL94 V-1 rated.This data was supplied by SABIC-IP for the Americas region.
Copyright © lookpolymers.com All Rights Reserved