Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.80 GPa | 406 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Uttap SF 600 Polyethersulfone Polyether Sulfone Resin-Medium Viscosity, unreinforced standard grade for Easy Injection Molding.Information provided by Ovation Polymers |
|||
Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYabs N30 ABS Information provided by Polykemi AB |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 |
Nilit Polynil® C50L Externally Lubricated PA66/6 Description: Polynil C50L shows better surface finish, flow and elongation than a comparable homopolymer. Key characteristics: Excellent flowHigh elongationGood impact strengthGood overall mechanica.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP J1000E PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000E is a compound based on PES resin. Added features include: Easy Moulding. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO 178 |
Nilit FRIANYL B63 W-KV10 Nylon 6 for injection molding, 10% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
Flexural Modulus | 2.80 - 25.0 GPa @Temperature -40.0 - 250 °C |
406 - 3630 ksi @Temperature -40.0 - 482 °F |
Average value: 9.10 GPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 |
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® BC 30 S 000000 Nylon 6 PA 6, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO 178 |
Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Dry) Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent .. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM-D790 |
Polyram RamTough PZ320G2 Polycarbonate, 10% Glass Fiber, Flame Retardant 10% glass fiber reinforced, flame retardant polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 2.80 GPa @Temperature 80.0 °C |
406 ksi @Temperature 176 °F |
ASTM D790 |
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D 790 |
Cossa Polimeri ESTADIENE 0615 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood impact resistance, stiff, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applic.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D 790 |
Cossa Polimeri ESTABIO PL 0560 T10 Biodegradable Plastic Biodegradable plastic for the extrusion of disposablesCertified for food contactInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO Data |
BASF Ultramid® 8202C HS PA6 (Dry) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 605 Nylon 6/6, PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO Data |
BASF Ultramid® 1003-2 NF2002 PA66 (Dry) Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | from bending test; DIN 53 457 |
Hippe PVC-U Polyvinyl Chloride Material at reasonable price, high strength. Used in machine construction as covers, pipes, section, façade elements.Information provided by Hippe. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO 178 |
Radici Heraform® R 3000 Acetal Copolymer Very easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Radici group. |