Mechanical Properties Metric English Comments
Flexural Modulus 2.828 GPa
410.1 ksi
ASTM D790
Lucent Polymers 66-01 Nylon 66, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 2.828 GPa
410.1 ksi
ASTM D790
Lucent Polymers POM-900P Acetal Homopolymer, Easy Flow, Injection Grade
Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 2.828 GPa
410.1 ksi
ASTM D790
Lucent Polymers POM-500 Acetal Homopolymer, General Purpose, Injection Grade
Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.