Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 20.1 GPa | 2920 ksi | ASTM D790 |
LNP Stat-Kon® LCL-4026 EM BK8-115 Polyetheretherketone, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(d Features: Electrically Conductive, Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discont.. |
|||
Flexural Modulus | 20.1 GPa | 2920 ksi | ASTM D790 |
LNP Lubricomp® OCL-4536 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant
(discontinu Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |