Flexural Modulus 20.8 GPa
3020 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI
LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive