Polymer Property : Flexural Modulus = 2069 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 14.27 GPa

@Thickness 3.20 mm
2069 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical