Mechanical Properties Metric English Comments
Flexural Modulus 21.4 GPa
3100 ksi
ASTM D790
LATI LARPEEK 10 K/30 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK)  (Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Flexural Modulus 21.4 GPa
3100 ksi
ASTM D790
Techmer ES HiFill® PA4/6 CF40 HS 40% Carbon Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites..
Flexural Modulus 21.4 GPa
3100 ksi
ASTM D790
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm
Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityAppearance: BlackProce..
Flexural Modulus 21.4 GPa
3100 ksi
ASTM D790
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm
Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant, UV Stabilized and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessing Method: Inject..