Polymer Property : Flexural Modulus = 21.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 21.9 GPa
3180 ksi
ASTM D790
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Crystalline  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..