Mechanical Properties Metric English Comments
Flexural Modulus 1.448 GPa
210.0 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Flex® TPO D-6507
Multi-Flex® D 6507 is a mineral filled TPO polypropylene compound designed for applications requiring high impact and moderate stiffness.Data provided by Multibase.
Flexural Modulus 1.448 GPa
210.0 ksi
ASTM D790
Eastman Tenite 360A4000012 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Flexural Modulus 1.448 GPa
210.0 ksi
ASTM D790
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Modulus 1.448 GPa
210.0 ksi
ASTM D790
Eastman Tenite 360E461312 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Modulus 1.448 GPa
210.0 ksi
ASTM D790
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp
Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st..
Flexural Modulus 1.448 GPa
210.0 ksi
ASTM D790
Eastman Tenite Propionate 375E4000012 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 1.448 GPa
210.0 ksi
ASTM D790
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 1.448 GPa
210.0 ksi
ASTM D790
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 1.448 GPa
210.0 ksi
ASTM D790
Eastman Tenite Propionate 383A2R30012 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 1.448 GPa
210.0 ksi
tangent; ASTM D790
Entec Hypro™ PPC-T10 Copolymer Polypropylene, 10% Talc Reinforced
Information provided by Entec
Flexural Modulus 1.448 GPa
210.0 ksi
ASTM D790
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..