Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.6 GPa | 2120 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66 LNP* STAT-KON* RE004 is a compound based on Nylon 66 resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 14.6 GPa | 2120 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXQ PEI LNP* THERMOCOMP* EC004XXQ is a compound based on Polyetherimide containing 20% Carbon Fiber. |
|||
Flexural Modulus | 14.6 GPa | 2120 ksi | ASTM D790 |
Plenco 6990 Phenolic, Briquette, Injection Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Flexural Modulus | 14.6 GPa | 2120 ksi | ISO 178-93 |
Wellman Wellamid® GF1750-BK1 50% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Flexural Modulus | 14.6 GPa | 2120 ksi | dry; ISO 178 |
DSM EcoPaXX® Q-HG10 PA410-GF50 50% Glass Reinforced, Heat Stabilized |