Mechanical Properties Metric English Comments
Flexural Modulus 0.910 - 147 GPa
132 - 21300 ksi
Average value: 13.8 GPa Grade Count:136
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..