Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.34 GPa | 2225 ksi | ASTM D790 |
PolyOne Lubri-Tech™ NL-30CF/15T Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedLow WearCarbon Fiber ReinforcedHigh StiffnessProcessing Method:MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |