Mechanical Properties Metric English Comments
Flexural Modulus 23.0 GPa
3340 ksi
ISO 178
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA)  (Unverified Data**)
Ixef 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-f..
Flexural Modulus 23.0 GPa
3340 ksi
Lehmann & Voss LUVOCOM® 1105-8002 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Flexural Modulus 23.0 GPa
3340 ksi
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea..
Flexural Modulus 23.0 GPa
3340 ksi
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
Flexural Modulus 23.0 GPa
3340 ksi
Lehmann & Voss LUVOCOM® 20-0659 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Flexural Modulus 23.0 GPa
3340 ksi
Lehmann & Voss LUVOCOM® 20-8171 Polyphthalamide, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Flexural Modulus 23.0 GPa
3340 ksi
Lehmann & Voss LUVOCOM® 1105/CF/30/EM PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Flexural Modulus 23.0 GPa
3340 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR
LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive.
Flexural Modulus 23.0 GPa
3340 ksi
ISO 178
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber
Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla..
Flexural Modulus 23.0 GPa
3340 ksi
ISO 178
Sumitomo Bakelite North America CF 9040A Carbon Fiber Reinforced Phenolic
CF 9040A is a high strength carbon fiber phenolic molding compoundInformation provided by Sumitomo Bak North America, Inc.
Flexural Modulus 23.0 GPa
3340 ksi
ASTM D790
Sumitomo Bakelite North America Epiall® 1904B-1 Short Glass Fiber Reinforced Epoxy
Epiall 1904B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided ..
Flexural Modulus 23.0 GPa
3340 ksi
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
Flexural Modulus 23.0 GPa
3340 ksi
DIN 53 457
Albis Plastics Tedur® L V 9404-1 PPS, 30% Carbon Fiber  (discontinued **)
High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fan Blades, Brake Sleeves, Model Constructi..