Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.165 GPa | 24.0 ksi | ASTM D790 |
Lubrizol Estane® ALR PC55D Thermoplastic Polyurethane Type: Estane® ALR PC60D is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
Flexural Modulus | 0.165 GPa | 24.0 ksi | ASTM D790 |
Lubrizol Estane® ALR PC60D Thermoplastic Polyurethane Type: Estane® ALR PC60D is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableInformation Provided by The Lubrizol Corporation |
|||
Flexural Modulus | 0.165 GPa | 24.0 ksi | ASTM D790 |
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based
(discontinued **) Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting e.. |