Flexural Modulus 16.77 GPa
2432 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA
LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant.