Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.700 GPa | 246.5 ksi | ASTM D790 |
Aclo Accuguard Polypropylene HP0369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Flexural Modulus | 1.700 GPa | 246.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436C40L Calcium Reinforced |
|||
Flexural Modulus | 1.700 GPa | 246.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437M20CL Mica Reinforced Coupled |
|||
Flexural Modulus | 1.700 GPa | 246.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C20L1 Calcium Reinforced |
|||
Flexural Modulus | 1.700 GPa | 246.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336W10L Wollastonite Reinforced |
|||
Flexural Modulus | 1.700 GPa | 246.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339C20L1 Calcium Reinforced |
|||
Flexural Modulus | 1.700 GPa | 246.5 ksi | ASTM D790 |
Aclo Accutech Polyethylene HD0234G10UVL High Density Glass Reinforced UV Stabilized |