Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 170 GPa | 24700 ksi | |
Kennametal Stellite Denertiaâ„¢ N19 Nickel Dental Alloy Denertiaâ„¢ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium freeInformation provided by Kennametal St.. |