Polymer Property : Flexural Modulus = 2480 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 17.1 GPa
2480 ksi
25 mm/min; ISO 178
PolyOne Nymax™ GF 1200 A 55 HS Natural Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Flexural Modulus 17.1 GPa
2480 ksi
ASTM D790
Sumitomo Bakelite North America FM 4004F Fiberglass and Mineral Reinforced Phenolic Novolac
FM 4004F is a fiberglass and mineral reinforced phenolic novolac compound with improved strength properties over FM 4004. This compound exhibits excellent dimensional stability and good strength at..