Mechanical Properties Metric English Comments
Flexural Modulus 25.58 GPa
3710 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON RE008 PA 66
LNP* STAT-KON* RE008 is a compound based on Nylon 66 containing 40% Carbon Fiber. Characteristics of this grade include: Electrically Conductive.