Flexural Modulus 3.86 - 17.5 GPa
560 - 2540 ksi
Average value: 10.1 GPa Grade Count:44
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..