Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.77 GPa | 256 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers MS 160 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
PolyMirae Moplen HP620M CPP Film Grade Polypropylene Moplen HP620M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP620M is suitable for rigid core resin of CPP. Moplen HP620M res.. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
PolyMirae Moplen HP640N Injection Molding Grade Polypropylene Moplen HP640N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640N is a homopolymer particularly suitable for injection molding.. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene Moplen HP740T is a nucleated polypropylene HOMO polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP740T is a homopolymer selected by customers for use in t.. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
I. Stern HIPS SH03 High Impact Polystyrene Features:High flowExcellent toughnessExcellent processabilityApplicationsInjection moldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co. Inc. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D760 |
LG Chemical SEETEC M1425 Polypropylene Impact Copolymer Features: SEETEC M1425 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1425 exhibits a very high stiffness and a good impact strength. SEETEC M1425 meets the FD.. |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HF5150H PP+MF15%, High Flow Description: Injection Molding, PP+MF15%, High FlowApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9160 ASA, Unreinforced Used in electric goods etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
Samyang Triloy® 130 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SH 03 High Impact Polystyrene Characteristics High flow Good melt strength Excellent toughness Processing MoldingApplications Gas assisted injection molding of T.V. cabinets Suitable for thin walled parts, AC grills and toys .. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 265 Toughened Polystyrene CharacteristicsGood clarity High dart impact strength High heat resistance Good stiffnessProcessing Extrusion Vacuum forming Applications Disposable glasses & bowls Deep draw formed products Ther.. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 266 Toughened Polystyrene CharacteristicsGood stiffness Excellent toughness High flow Excellent clarity Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric instruments .. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 566 Flame Retardant Polystyrene Characteristics Good flow and toughness Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Available in any color Processing Extrusion MoldingApplications Large size T.V. Cabinets El.. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 6131 XF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 8515 TY Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 8005 DW Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 8015 FRC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
Entec Hyrene® PS-HI 14/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron PT-45M ABS Antistatic Extrusion Grade Antistatic Cop Sleeves ApplicationInformation provided by Bhansali |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP EXP 31 Toughened Polystyrene Characteristics Very high clarity & gloss High dart impact strength & good stiffness Good crease retention Good heat resistance High yield compared to PVC, APET Processing Extrusion Vacuum form.. |