Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.658 GPa | 2561.1 ksi | ASTM D790 |
E-Polymers SEPAZ® LA60 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |