Polymer Property : Flexural Modulus = 26.5 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 26.5 GPa
3840 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX04522C PC (Asia Pacific)
LNP Stat-Kon DX04522C is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: High Modulus, Electrically Conductive, Clean Compound System. Also ..
Flexural Modulus 26.5 GPa
3840 ksi
longitudinal; ISO 178
Bond Laminates TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact ..