Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.834 GPa | 266.0 ksi | ASTM D790 |
RedEye On Demand ABS for Rapid Prototyping ABS or Acrylonitrile butadiene styrene is a true industrial thermoplastic that is impact-resistant and structurally strong. ABS parts are built with a layered manufacturing process utilizing Fused D.. |
|||
Flexural Modulus | 1.834 GPa | 266.0 ksi | ASTM D790 |
Stratasys® ABS ABS is a strong, durable production-grade thermoplastic used across many industries. ABS is an ideal material for conceptual prototyping through design verification through direct digital manufactur.. |