Mechanical Properties Metric English Comments
Flexural Modulus 1.08 - 27.5 GPa
156 - 3990 ksi
Average value: 10.6 GPa Grade Count:34
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..