Mechanical Properties Metric English Comments
Flexural Modulus 0.00300 - 0.190 GPa
0.435 - 27.6 ksi
2% Secant; ASTM D790
Dow Engage® Polyolefin Elastomer
Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. ..