Flexural Modulus 1.931 GPa
280.1 ksi
ASTM D790-1
Ineos Styrenics Avantra® 525K High Impact Styrenic Polymer (NAFTA)
Description: Specialty and super-high impact grades for a variety of applications such as refrigerator liners, consumer electronics housings, recreation equipment and sporting goods, toys, office pr..
Flexural Modulus 1.931 GPa
280.1 ksi
ASTM D790
Lucent Polymers CPP-120 Polypropylene Homopolymer, 20% Calcium Carbonate Filled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.931 GPa
280.1 ksi
ASTM D790
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate
Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 1.931 GPa
280.1 ksi
ASTM D790
Proto3000 PC-ABS Fused Deposition Modeling Polymer
Description: PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior strength and heat resis..