Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.966 GPa | 285.1 ksi | ASTM D790 |
Ineos Nova 5540 High Impact Polystyrene
(discontinued **) Excellent balance of toughness, flow, and set-up, High gloss, USP Class VIApplications: Structural foam, Housewares, Toys, Appliance parts, Dairy containersProperties were determined on injection mo.. |